| 王道文,史晓冬.横管连蒸制浆系统中蒸煮管壁减薄的原因分析[J].中国造纸,2011,30(2):38-40 |
 二维码(扫一下试试看!) |
| 横管连蒸制浆系统中蒸煮管壁减薄的原因分析 |
| Analysis of the Thinning of the Wall of the Cooking Tube in a Continuous Digestor |
| 收稿日期: |
| DOI:10.11980/j.issn.0254-508X.2011.02.009 |
| 关键词: 蒸煮管 减薄 磨损 腐蚀 |
| Key Words:cooking tube thinning wear corrosion |
| 基金项目: |
|
| 摘要点击次数: 8386 |
| 全文下载次数: 3029 |
| 摘要:介绍了某纸厂150 t/d以棉秆为原料的连蒸系统中蒸煮管的现场检验情况,分析了棉秆连蒸系统中蒸煮管全面减薄的原因,并提出了相应的对策。 |
| Abstract:The reason of overall thinning of the cooking tube in a horizontal continuous digestor using for cotton stalk pulping with 150 t/d capacity was analyzed, the corresponding solutions were discussed. |